Are you sure that is that is every word Robert said? It does not sound right to me. Sacrificial Anode is for corrosion protection, which is the opposite phenomena of scaling. In fact, when you have scaling, the sacrificial anode is no use.

Scaling causes are from nucleation surface and saturation of mineral. A slick non metal surface like WDRP would help, but for hard water you still experience scaling more or less.