It's not just the size but also the shape of the powder particles. Spherical particles lead to fewer voids but most voids are caused by [the low percentage of] hollow particles in the Arcam powder. Spherical voids do distribute stress better than voids with sharp corners but it's still best to remove any voids with HIP or complex die-forge methods.

www.sciencedirect.com/science/article/pii/S104458031500039X

There's a paper out there somewhere showing fewer defects with the small spherical particles that Arcam produces. Couldn't find it just now.